Influence of the Equal Channel Angular Pressing(ECAP) processing on stress corrosion cracking (SCC) of AA5083 aluminium alloy

Asiful H. Seikh, Centre of Excellence for Research in Engineering Materials, Deanship of Scientific Research, King Saud University, Saudi Arabia.

Aluminium (Al) alloy is the most useful material for several technological purposes, mainly due to the good combination of intermediate-to-high mechanical strength with low density, good formability and high stress corrosion cracking resistance. In this present work a severe plastic deformation through equal channel angular pressing (ECAP) upto three passes was given on Al5083 alloy using route-BC at room temperature. Stress Corrosion Cracking (SCC) resistance was evaluated by 10-4/sec strain rate and the constant load tests performed in an aqueous environment of 3.5 wt.% NaCl. For more understand on the SCC susceptibilities of the Al alloy shown by the ECAPed and as received samples, microstructural characterization was carried out of the fracture surfaces by SEM (Scanning Electron Microscopy) and EBSD (Electron Back Scattered Diffraction). Improvement of the SCC resistance of the Al alloy subjected to 1st pass of the ECAP compared to the as-received Al alloy but after 2nd and 3rd   passes susceptibility of SCC reduces. The dimple of the fracture surface after 1st pass of the ECAPed Al samples is shown finest type, that is shown to the best ductility of Al samples. The propagation of the cracks towards the grain boundaries with {100}//RP orientation of the grains and the grain boundaries related to {111}//RP and {110}//RP orientated grains slowed down the SCC of the Al alloy.

மறுப்பு: இந்த சுருக்கமானது செயற்கை நுண்ணறிவு கருவிகளைப் பயன்படுத்தி மொழிபெயர்க்கப்பட்டது மற்றும் இன்னும் மதிப்பாய்வு செய்யப்படவில்லை அல்லது சரிபார்க்கப்படவில்லை.